Global NM-3255 High Density Polyethylene, Yarn/Tape Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , HDPE, Fiber Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Global NM-3255 High Density Polyethylene, Yarn/Tape Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing nets, wire & cable insulators, auto parts, pipesInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D792
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.0 MPa
6240 psi
ASTM D638
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break 2000 %
2000 %
ASTM D638