Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® IG464-C Injection Molded HDPE Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® IG464-C Injection Molded HDPE Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
IG464-C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG464-C is subject to the specific limitation that it may contact food only at temperatures of 212°F and below.NOVA Chemicals' polyethylene resins are chemically and biologically inert.Features: Superior stiffness allows for part thinwalling and enhanced stacking strength, Low viscosity for exceptional processability yielding shorter cycle times and energy savings, Exceptional physical properties provide impact resistance for demanding applications, Low warpage for improved part quality and reliabilityAdditives: AntioxidantApplications: Crates, Pallets, Totes, Pails
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
50 mm/min test speed; ASTM D 638
Tensile Strength, Yield 27.0 MPa
3920 psi
50 mm/min test speed; ASTM D 638
Elongation at Break 1250 %
1250 %
50 mm/min test speed; ASTM D 638
Elongation at Yield 8.0 %
8.0 %
50 mm/min test speed; ASTM D 638
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM D 790
Users viewing this material also viewed the following: