Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP66GF15 Nylon 66, 14% Glass Reinforced Nylon 66 - Glass reinforced (14 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ISO 527 |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1000FC PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. NSF-51 certified for selected colors. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010K PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 4002 PEI PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQNH4550 PBT Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF/B40 L 40% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 40% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: Natural ColorInformation provided by TP.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF/M30 HS BK 10/20% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral Filler, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | |
Alcoa MIC-6 Aluminum Mold Alloy MIC-6 is a blend of the most desirable features of many individual metals. The result is a cast aluminum plate that meets the challenge of product accuracy demanded by today’s industry.Because of i.. |
|||
Tensile Strength, Yield | 105 MPa @Strain 0.200 % |
15200 psi @Strain 0.200 % |
|
ALIMEX ACP 6000 Aluminum Cast Plate Aluminum cast plate ACP 6000 is a 7xxx series alloy surface-machined plate. This type of alloy ensures excellent machinability characteristics and adequate tensile strength. Thickness, flatness and .. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | ASTM D638 |
Beijing Ranger Chem PBT-201-G15 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |
|||
Tensile Strength, Yield | 105 MPa | 15200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |