Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Opnyl OP66GF15 Nylon 66, 14% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ovation Polymers
Trade Name Opnyl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Opnyl OP66GF15 Nylon 66, 14% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nylon 66 - Glass reinforced (14 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm

@Thickness 3.17 mm
0.0050 - 0.0080 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.0060 - 0.011 cm/cm

@Thickness 3.17 mm
0.0060 - 0.011 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 105 MPa
15200 psi
50 mm/min; ASTM D638
Elongation at Break 3.5 %
3.5 %
50 mm/min; ASTM D638
Tensile Modulus 4.10 GPa
595 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 135 MPa
19600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4.30 GPa
624 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 238 °C

@Thickness 3.20 mm
460 °F

@Thickness 0.126 in
unannealed; ASTM D648