Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
LG Chemical LG-749 ABS, Low Gloss, High Heat Resistance Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styron Magnumâ„¢ 3453 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3453 ABS is a general purpose injection molding resin suitable for a wide range of applications.Information provided by DowThis product line was spun off from Dow Chemical to Styron in .. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F6RY01 Nylon 6, 30% Glass Fiber SAXAMID 126F6RY01 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -20.0 °C |
4.28 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -40.0 °C |
4.28 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -20.0 °C |
4.28 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide AG6H PA66, 30% Glass Filled, Injection Molded AG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -20.0 °C |
4.28 ft-lb/in² @Temperature -4.00 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -20.0 °C |
4.28 ft-lb/in² @Temperature -4.00 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -20.0 °C |
4.28 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR20 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR25 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR30 NL PBT 30% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecopet® PT74 GR45 BK002 PR PET, 45% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) Zytel® BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature -40.0 °C |
4.28 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66 Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Izod Impact, Notched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |