Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Qualchem Danamid AFES-21 Polyamide 66 Impact resistant, dryInformation provided by Qualchem Zrt. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1162T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXM3729 PC (Europe-Africa-Middle East) LEXAN FXM3729 is an UV stabilized Visual FX Sparkle grade, with an excellent flow. It contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® IM1063 PC (Europe-Africa-Middle East) Lexan* IM1063 is a impact modified polycarbonate gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -20.0 °C |
26.2 ft-lb/in² @Temperature -4.00 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade) Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -20.0 °C |
26.2 ft-lb/in² @Temperature -4.00 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -20.0 °C |
26.2 ft-lb/in² @Temperature -4.00 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem UR9076LG PEI Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Luran® S KR2866C ASA / PC Luran S KR2866C is a blend of ASA and PC with a reduced content of PC. It is characterized by a medium impact toughness and heat resistance.Good heat resistanceMedium impact strengthInformation prov.. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -40.0 °C |
26.2 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Polyram RamLloy PZF101 PC/PBT Alloy, Chemical Resistance PC/PBT alloy for injection molding applications, low temperature and chemical resistance.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature -40.0 °C |
26.2 ft-lb/in² @Temperature -40.0 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL IM PA6, impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® PC40 NL VB02 PC, unfilled, UV stabilized, high impact, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |