Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1A
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibersInformation provided by LANXESS.
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 80
LG Chemical HF-350 ABS, High Flow, High Impact
Information Provided by LG Chem
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1A
Ineos ABS Lustran® ABS 680 LNS503 High Performance Injection Molding Grade
Lustran® ABS 680 LNS503 is an easy flow version. It is a high performance injection molding grade used for refrigerator and freezer door end caps.
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1A
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade
Lustran® Ultra 4000 PG is electroplating grade with high heat resistance. It is used for the production of molded plastic articles.
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styrolution Novodur® 4000PG ABS
Novodur Ultra 4000PG is an injection molding grade especially suitable for electroplating, providing enhanced heat resistance.Information provided by Styrolution
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1A
Styrolution Novodur® P2M-AT ABS Pellets
Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles.
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1A
Styrolution Novodur® P2M-V ABS Pellets
Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles.
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS)
MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun ..
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers
Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch..
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature -20.0 °C
10.9 ft-lb/in²

@Temperature -4.00 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66  (Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature -10.0 °C
10.9 ft-lb/in²

@Temperature 14.0 °F
ISO 180
Dow INSPIRE™ 112 Performance Polymer
INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, Conditioned
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer
Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion ..
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified
SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties...
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180