Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East) CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy EXGY30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CB259 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB259 medium high melt flow, 1,600 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact r.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 0.000 °C |
1.43 ft-lb/in² @Temperature 32.0 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ TKS708D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TKS708D medium high melt flow, 1,300 MPa flexural modulus, UV-stabilized, high impact thermoplastic elastomeric olefin (TEO) resin has an excellent combination of propert.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ XFBR712 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ XFBR712 medium melt flow, 1,800 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness, impact resistance.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 1760T PBT+PC (Europe-Africa-Middle East) XENOY 1760T is developed as a easy flow material, for applications such as doorhandles and mirror housings. It is a 11% glass reinforced material with excellent strength and dimensional stability.Th.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1A |
Domo 2300L Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide A28N PA66, Nucleated, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide A28N PA66, Nucleated, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 179/1eA |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GB20 NL PBT, 20% glass bead reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam EXCP0132 PA, Mineral Filled, Injection Molding Starflam EXCP0132 is a Halogen Free and Red Phosphorous Free, Mineral Filled, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecolen® HP30 NL XC30 PPHP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
Polykemi AB POLYfill PPH T5040 FC Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
ISO 180/4A |
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |