Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP OCL36XXP PPS - Linear (Europe-Africa-Middle East) LNP* LUBRICOMP* OCL36XXP is a compound based on PPS- Linear resin containing PTFE, Carbon Fiber. Added features include : Internally Lubricated, Electrically Conductive . |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 (Asia Pacific) LNP* STATKON* RFD03 is a compound based on PA 66 resin contaning Carbon Powder, Glass Fiber. Added features include: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP KF002 Acetal Copolymer LNP THERMOCOMP* KF002 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East) 10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP AW00A ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AW00A is a compound based on Acrylonitrile Butadiene Styrene resin containing Wollastonite. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180-93 |
Wellman EcoLon® MRGF1914-BK1 Nylon 66, 40% Mineral and Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® 42LN2-N Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® MRGST1715-WBK1 Nylon 6, 25% Mineral and Glass Sphere Reinforced, Impact Modified, Weatherable Grade All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -40.0 °C |
2.38 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® B3S HP PA6 (Dry) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 218 S30 is used in all sectors of indu.. |