Polymer Property : Izod Impact, Notched (ISO) = 6.50 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/A
Victrex® HT™ P45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, co..
Izod Impact, Notched (ISO) 6.50 - 10.0 kJ/m²
3.09 - 4.76 ft-lb/in²
Average value: 8.09 kJ/m² Grade Count:4
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Iran Petrochemical (PCC) EPD 60 R Polypropylene
EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include t..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Iran Petrochemical (PCC) S 30 S Polypropylene
This grade is for general injection molding applications.Applications: textile bobbins ,wheels ,fittings ,closures ,caps.Information provided by Iran Petrochemical Commercial Co.
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
Lushan PP+GF30% Maleic Anhydride Grafted Polypropylene
Malic anhydride grafted polypropylene (PP-a-MAH) Lushan series is evaluated as compatiblizer/coupling agent which is used to fill or reinforced polypropylene. As the coupling agent, PP-g-MAH can sig..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Iran Petrochemical (PCC) EPV 31 RA Polypropylene
A high fluidity heterophasic copolymer for thin wall injection molding exhibits high stiffness, relatively good impact residence.Applications: flower pots, containers, filters, house wares.Informati..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Iran Petrochemical (PCC) S 28 F Polypropylene Film
Biaxially oriented poly propylene films suitable for metallization Applications: cosmetics , food stuffs , lamination and other flexible films.Information provided by Iran Petrochemical Commercial C..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Iran Petrochemical (PCC) S 30 G Polypropylene
The grade has combined excellent process ability with high stiffness.Applications: bags, mats, packing twines and ropes, drinking beakers packaging for dairy products.Information provided by Iran Pe..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/1A
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Polyram PlusTek PA350M4 Nylon 6.6 for Injection Molding, 20% Mineral Reinforced
20% Mineral Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ASTM D256
Tipco Tipcofil® AG 300 - 15% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability
15% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Tisan TISLAMID® 6 UNR Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180-93
Wellman Wellamid® GF25-60 XE-NBK1 25% Glass Fiber Reinforced Nylon 6
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding
Total Petrochemicals PPR 9220 is a nucleated random copolymer polypropylene with a melt flow index of 20 g/10 min for the injection molding of articles with high transparency and excellent surface a..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ASTM D256
Total PS CPDS 850S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 850S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ASTM D256
Total PS CPDS 855S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 855S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ASTM D256
Total PS CPDS 856S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 856S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ASTM D256
Total PSI 2451 High Heat Resistance Impact Polystyrene
Total Petrochemicals Polystyrene 2451 is a high heat resistance, impact polystyrene for injection blow molding, thermoforming. It is recommended for the manufacturing of articles which require good..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/1A
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
1A; ISO 180
Azoty Tarnow™ TARNOFORM 300 K POM
Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
1A; ISO 180
Azoty Tarnow™ TARNOFORM 300 XEC1 POM
Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe ..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO Test
BASF Ultraform N 2320 U03 UNC Q600 POM
Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade.
Izod Impact, Notched (ISO) 6.50 kJ/m²

@Temperature 23.0 °C
3.09 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/A
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
Izod Impact, Notched (ISO) 6.50 kJ/m²

@Temperature 23.0 °C
3.09 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/A
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/A
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry)
ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase..
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Polyram RamOfin PPC343T4 Polypropylene, 20% Mineral Filled
20% Mineral filled, UV stabilized, heat stabilized polypropylene for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/A
Victrex® HT™ P45PF Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor..