Material Notes:
Biaxially oriented poly propylene films suitable for metallization Applications: cosmetics , food stuffs , lamination and other flexible films.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 2.0 g/10 min
2.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ISO 868
Tensile Stress 35.0 MPa
5080 psi
ISO R527
Elongation at Yield 13 %
13 %
ISO R527
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 155 °C
311 °F
ISO 306/A
Heat Distortion Temperature 105 °C
221 °F
ISO 75/B