Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/3A |
PolyOne Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66) The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ah.. |
|||
Izod Impact, Notched (ISO) | 3.50 - 6.50 kJ/m² @Thickness 4.00 - 4.00 mm |
1.67 - 3.09 ft-lb/in² @Thickness 0.157 - 0.157 in |
Average value: 5.75 kJ/m² Grade Count:7 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | Low Temp; DIN 53453 |
Ineos Nova S-4200 Medium Impact Compact Polystyrene
(discontinued **) Medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical.. |
|||
Izod Impact, Notched (ISO) | 3.50 - 60.0 kJ/m² | 1.67 - 28.6 ft-lb/in² | Average value: 17.0 kJ/m² Grade Count:27 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Notched (ISO) | 3.50 - 861 kJ/m² | 1.67 - 410 ft-lb/in² | Average value: 33.0 kJ/m² Grade Count:39 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-1A |
Gromax BPR20-N1 Nylon 6, Flame Retardant (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO Test |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO Test |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® FPT 20 - 20% Talc Reinforced Polypropylene Homopolymer Compound 20% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman EcoLon® MR1660-BK1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180 |
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GS40-60 42L-NBK1 40% Glass Sphere Reinforced Nylon 6 Description: Glass Sphere Reinforced Nylon 6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® MRGF3820-N 38% Mineral/Glass Reinforced Developmental Grade Nylon 66 Description: Mineral/Glass Reinforced Developmental Grade Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman Wellpet® PR118-N2 Unfilled Polyester PET Description: Unfilled Polyester PETInformation provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 9082 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9082 is a controlled-rheology and antistatic homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing impr.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 9089 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9089 is a very low molecular weight distribution homopolymer propylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9089 is intended for the ex.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® PP FR V0 - UL94-V0 Flame Retardant Polypropylene Homopolymer V-0 Flame Retardant PP HomopolymerApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness >=5.00 mm |
1.67 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit IIQ Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness >=5.00 mm |
1.67 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit IR Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity. Very low water absorption.Application:.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Crastin® 6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin 6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont .. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 500 GB6 POM 30% glass beads filled low viscosity grade with very high stiffness and hardness with lowered shrinkage combined with easy molding of complicated shapesInformation provided by Zakłady Azotowe w .. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 542 Polypropylene Homopolymer Unreinforced, high heat resistance, antistaticInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene J 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl A2 ZG30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene PMD 50203 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |