Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC
LNP* LUBRICOMP* DFL36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
ISO 180/U
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DFL-4036 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXP PC
LNP* Lubricomp* DFL36XXP is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 55.0 - 60.0 kJ/m²

@Temperature -30.0 - -30.0 °C
26.2 - 28.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 57.5 kJ/m² Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Izod Impact, Unnotched (ISO) 55.0 kJ/m²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1U
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 (Europe-Africa-Middle East)
LNP* Verton* RL002 is a compound based on Nylon 66 resin containing PTFE.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRILOY RF208 PA 66
LNP LUBRILOY* RF208 is a compound based on Nylon 66 resin containing 40% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRILOY RF208 PA 66 (Asia Pacific)
LNP LUBRILOY* RF208 is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East)
VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo..
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific)
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF004ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP PF006 PA 6
LNP THERMOCOMP* PF006 is a compound based on Nylon 6 resin containing 30% Glass Fiber.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP UF008AR PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF008AR is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF VF004S SUPER TOUGH NYLON (Europe-Africa-Middle East)
LNP* THERMOTUF* VF004S is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Izod Impact, Unnotched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP IP004Z PA6.12 (Europe-Africa-Middle East)
LNP* LUBRICOMP* IP004Z is a compound based on PA 6/12 resin containing PTFE, Silicone. Added features include : Internally Lubricated, Extrusion grade.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East)
VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermotuf PF007IX2 PA 6 (Europe-Africa-Middle East)
LNP * THERMOTUF* PF007IX2 is a compound based on PA 6 resin containing Glass Fiber. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific)
PPE+PS, HDT 125
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar.
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
ISO 180/1C
Chi Mei Polylac® PA-758R ABS - Transparent
Transparent, Chemical Resistant
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
50%RH; ISO 180/1U
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT 403 M-G15 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
ASTM D256
BLUESTAR 201G25 PBT, 25% Glass Filled
Typical Applications: Energy saving lightingInformation provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-201-G20 211 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
DAM; ISO 180/1U
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p..
Izod Impact, Unnotched (ISO) 55.0 - 67.0 kJ/m²

@Temperature -30.0 - -30.0 °C
26.2 - 31.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 61.0 kJ/m² Grade Count:2
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Copyright © lookpolymers.com All Rights Reserved