Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East) LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat. |
|||
Izod Impact, Unnotched (ISO) | 35.0 - 67.0 kJ/m² @Temperature -30.0 - -30.0 °C |
16.7 - 31.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 52.8 kJ/m² Grade Count:5 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 - 100 kJ/m² | 16.7 - 47.6 ft-lb/in² | Average value: 58.9 kJ/m² Grade Count:12 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 35.0 - 48.6 kJ/m² | 16.7 - 23.1 ft-lb/in² | Average value: 39.4 kJ/m² Grade Count:4 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KP004 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP LCL36 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL36 is a compound based on Polyetheretherketone containing Carbon Fiber , PTFE. Added features of this material include Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE... |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF002S is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MF004S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF004S is a compound based on Polypropylene resin, containing Glass Fiber. Added features include; Chemically Coupled.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Izod Impact, Unnotched (ISO) | >= 35.0 kJ/m² | >= 16.7 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.3 |
Hippe UP GM 202 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant.Information provid.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam PX06010 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06010 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RFM3353EM PA66/6, Glass/Mineral Fiber Reinforced, Injection Molding Starflam RFM3353EM is a Mineral Filled, Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |