Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 18.0 - 41.0 kJ/m² | 8.57 - 19.5 ft-lb/in² | Average value: 30.5 kJ/m² Grade Count:8 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 - 20.0 kJ/m² | 8.57 - 9.52 ft-lb/in² | Average value: 19.3 kJ/m² Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
8.57 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 31.0 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 - 100 kJ/m² @Temperature -30.0 - -30.0 °C |
8.57 - 47.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 67.0 kJ/m² Grade Count:4 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI (Europe-Africa-Middle East) LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 LNP* STAT-KON* RFD03 is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON ZE0039 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP 9X07435 LNP* THERMOCOMP* is a compound based on Miscellaneous resin containing Proprietary Filler(s). Added feature of this grade is: Plateable. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific) LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NC180A Homopolymer 15% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NCQAG Copolymer 40% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NCTAG Copolymer 50% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR LNP* STAT-KON* OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180A |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi.. |