Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* STAT-KON* OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Density 1.377 g/cc
0.04975 lb/in³
ASTM D792
Moisture Absorption 0.0100 %
0.0100 %
50% RH, 24 hrs; ASTM D570
0.0200 %
0.0200 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm

@Time 86400 sec
0.0050 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cm

@Time 86400 sec
0.0060 - 0.0090 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
Type I, 5 mm/min; ASTM D638
96.0 MPa
13900 psi
5 mm/min; ISO 527
Tensile Strength, Yield 95.0 MPa
13800 psi
Type I, 5 mm/min; ASTM D638
96.0 MPa
13900 psi
5 mm/min; ISO 527
Elongation at Break 1.7 %
1.7 %
5 mm/min; ISO 527
1.7 %
1.7 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 1.7 %
1.7 %
5 mm/min; ISO 527
1.7 %
1.7 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 7.39 GPa
1070 ksi
5 mm/min; ASTM D638
7.50 GPa
1090 ksi
1 mm/min; ISO 527
Flexural Strength 142 MPa
20600 psi
1.3 mm/min, 50 mm span; ASTM D790
148 MPa
21500 psi
ISO 178
Flexural Yield Strength 141 MPa
20500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.44 GPa
934 ksi
1.3 mm/min, 50 mm span; ASTM D790
6.52 GPa
946 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.330 J/cm
0.618 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.91 J/cm
5.45 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 7.00 J

@Temperature 23.0 °C
5.16 ft-lb

@Temperature 73.4 °F
ASTM D3763
Impact Test 1.00 J
0.738 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
28.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 259 °C
498 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
263 °C

@Thickness 3.20 mm
505 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
252 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
189 °C

@Thickness 3.20 mm
372 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 3.0 - 6.0 ohm
3.0 - 6.0 ohm
ASTM D257