Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GF 30 HI PA66, 30% glass fibre, improved strength FeaturesPA 66 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RV300LK (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -40.0 °C |
45.2 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S223-PG6U (Dry) 33% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **)& Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eU |
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Suzhou Hipro Polymers Hiprolon® 200 MC HLS G30 Nylon 1010, 30% glass fiber filled Hiprolon® 200 MC HLS G30 is a polyamide 10.10 compound reinforced with 30% chopped glass fiber for injection molding; features high dimension stability, chemical resistance, impact resistance, lo.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-G6U (Dry) 33% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Akulon® K224-G8 PA6-GF40 40% Glass Reinforced |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-HG6U (Dry) 33% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecomid® NB40 GR30 NL PA 6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K-FG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
(Unverified Data**) Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po.. |
|||
Charpy Impact Unnotched | 9.50 J/cm² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecomid® NB40 GR30 NL IH PA 6 30% glass fiber reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |