Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 97.0 MPa @Thickness 4.00 mm, Temperature 23.0 °C |
14100 psi @Thickness 0.157 in, Temperature 73.4 °F |
ISO 527-2/5 |
PolyOne Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 10mm/min; ASTM D638 |
Kingfa JH720 G20 20% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD.. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, Conditioned Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features include: Exceptional Processing, Non-Brominated & Non-Chlorinated Flame Retardant. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC (Asia Pacific) LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing, Flame Retardant, Non-Br.. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF003H PA 66 LNP* THERMOCOMP* RF003H is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF003XXH PA 66 LNP* THERMOCOMP* RF003XXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp ZF008 PPO LNP* Thermocomp* ZF008 is a compound based on Modified PPO containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP ZF004 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004 is a compound based on PPE+PS Blend resin containing Glass Fiber. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | Conditioned; ISO 527 Type 1 A |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ISO 527-93 |
Wellman Wellamid® MRGFX1716-BK1 40% Mineral/Glass Reinforced, Silicone Lubricated Nylon 6 Description: Mineral/Glass Reinforced, Silicone Lubricated Nylon 6Information provided by Wellman. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ISO 527; DIN 53455 |
Zell-Metall Engineering Plastics Zellamid 1500 (PEEK) Zellamid® 1500 (Polyetheretherketone - PEEK, natural) is the registered trademark for Zell-Metalls semi-crystalline high performance thermoplastic which exhibits a unique combination of high m.. |
|||
Tensile Strength at Break | 97.0 MPa @Temperature 23.0 °C |
14100 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 515CS BK575M PET Rynite® 515CS BK575M is a 15% glass fiber reinforced, black polyethylene terephthalate resin modified for improved color stability after heat aging.Information provided by DuPont Performance Polyme.. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ISO 527 |
BASF Petra® 7010 BK 5830 15% Glass Filled PET Description: Petra 7010 BK5830 is a 15% glass fiber reinforced, pigmented black injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Tensile Strength at Break | 97.0 MPa @Temperature 80.0 °C |
14100 psi @Temperature 176 °F |
ISO Data |
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat
cushion .. |
|||
Tensile Strength at Break | 97.0 MPa | 14100 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester, TP (Asia Pacific) LNP* THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Mineral, Glass Fiber. Added features of this material include: Flame Retardant. |