Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized and provides optimized injection moulding performance. This product is available in natural, grey & black colors as standard and can be made in other specific colors upon request.Benefits: This product offers excellent flame retardancy properties (UL 94, 5VA, GWIT) combined with best in class processing, mechanical and electrical performance.Available in: Asia Pacific, Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: This product is ideally suited for power distribution, industrial control and appliance applications such as MCBs and contactors, as well as being able to be used in many varied thin wall applications where its high flow polymer base enables it to achieve a UL94 V-0 rating down to a 0.4mm wall thickness.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 97.0 MPa
14100 psi
ISO 527 Type 1A
Elongation at Break 5.1 %
5.1 %
ISO 527 Type 1A
Tensile Modulus 8.50 GPa
1230 ksi
ISO 527 Type 1A
Flexural Strength 175 MPa
25400 psi
ISO 178
Flexural Modulus 7.10 GPa
1030 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 63.0 kJ/m²
30.0 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.25 J/cm²
5.95 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 212 °C
414 °F
ISO 75/Af
Electrical Properties Metric English Comments
Dielectric Constant 4.35
4.35
IEC 60250
Dielectric Strength 23.0 kV/mm
584 kV/in
IEC 60243
Dissipation Factor 0.080
0.080
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 220 - 225 °C
428 - 437 °F
Front Barrel Temperature 240 - 245 °C
464 - 473 °F
Mold Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 235-240°C
Copyright © lookpolymers.com All Rights Reserved