Polymer Property : Charpy Impact Unnotched = 1.60 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
Polimeri Europa KOSTIL B366 Styrene Acrylonitrile
Symbol according to ISO 1043-1: SAN Grade designation according to ISO 4894-SAN 2,M,105-25 Injection moulding grade with good chemical resistance and easy flow grade Application fields: household..
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
Polimeri Europa KOSTIL B366 Styrene Acrylonitrile
Symbol according to ISO 1043-1: SAN Grade designation according to ISO 4894-SAN 2,M,105-25 Injection moulding grade with good chemical resistance and easy flow grade Application fields: household..
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -40.0 °C
7.61 ft-lb/in²
<br>@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled
Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding
Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.60 - 4.20 J/cm²
7.61 - 20.0 ft-lb/in²
Average value: 2.80 J/cm² Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Charpy Impact Unnotched 1.60 - 4.20 J/cm²
<br>@Temperature -40.0 - -20.0 °C
7.61 - 20.0 ft-lb/in²
<br>@Temperature -40.0 - -4.00 °F
Average value: 2.70 J/cm² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 50-8376 Polycarbonate, unreinforced
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical engineering.Antistatic.Isotropic shrinkage characteristics.Reduced moment..
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6
Description: TECHNYL B 52 G1 MX35 is a copolyamide 6.6/6 , with thermal protection, glow wire resistant and reinforced with mineral filler.Colors: GreyAvailable in: Latin AmericaMain Properties: ? G..
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179
Styrolution Luran® 358 N SAN
Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
Styrolution Luran® 358 N SAN
Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179
Styrolution PS 454N HIPS
Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss..
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Dry)
Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No ..
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
BASF Novolen® 1040 K Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade
Injection molded parts, film tape, fibrillated film and monofilaments.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
BASF Novolen® 1184 L Polypropylene
Nucleated grade with high processing stability containing antistatic for thermoformed parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
BASF Novolen® 3200 MC Polypropylene
Cast film without slip and blocking agents.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature -30.0 °C
7.61 ft-lb/in²
<br>@Temperature -22.0 °F
BASF Novolen® 1102 L Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.60 J/cm²
<br>@Temperature 23.0 °C
7.61 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/2C
SABIC Innovative Plastics Noryl FN215D PPE+HIPS (Europe-Africa-Middle East)
NORYL FN215 is a Noryl Engineering structural foam grade fulfilling a wide range of application requirement. Moulded with the recommended blowing agents, this material provides all the performance r..
Charpy Impact Unnotched 1.60 - 7.50 J/cm²
7.61 - 35.7 ft-lb/in²
Average value: 4.16 J/cm² Grade Count:7
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..