Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66 Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -40.0 °C |
12.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HH-TFGV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -40.0 °C |
12.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 H-SG50 Nylon 6.6 for injection molding, 50% mineral filled Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -40.0 °C |
12.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 SG-GV 2010 Nylon 6.6 for injection molding, 20% mineral filled and 10% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² | 12.8 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL B63 BR90 Nylon 6.6 for injection molding, 90% bronze filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -40.0 °C |
12.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² | 12.8 ft-lb/in² | DIN 53453 |
Nilit RECONYL B GV30 Recycled nylon 6 for injection molding, 30% glass fiber reinforced Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -40.0 °C |
12.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -40.0 °C |
12.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 TF-KV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -40.0 °C |
12.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled and 10% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -40.0 °C |
12.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit RECONYL B KV30 Recycled nylon 6 for injection molding, 30% glass ball reinforced Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.70 - 5.50 J/cm² | 12.8 - 26.2 ft-lb/in² | Average value: 4.17 J/cm² Grade Count:10 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 2.70 - 6.00 J/cm² @Temperature -40.0 - -30.0 °C |
12.8 - 28.6 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.42 J/cm² Grade Count:10 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eU |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² | 12.8 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, Conditioned Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature -30.0 °C |
12.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Charpy Impact Unnotched | 2.70 J/cm² @Temperature 23.0 °C |
12.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® SK612SF BK591 PBT Crastin® SK612SF BK591 is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast .. |
|||
Charpy Impact Unnotched | 2.70 J/cm² | 12.8 ft-lb/in² | ISO 179/1eU |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² | 12.8 ft-lb/in² | ISO 179 |
Teijin Panlite® BS-8110R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Charpy Impact Unnotched | 2.70 - 6.00 J/cm² | 12.8 - 28.6 ft-lb/in² | Average value: 3.82 J/cm² Grade Count:12 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact Unnotched | 2.70 J/cm² | 12.8 ft-lb/in² | |
LATI Latilub 88/10-15T K/30 PEEK, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Charpy Impact Unnotched | 2.70 - 7.00 J/cm² | 12.8 - 33.3 ft-lb/in² | Average value: 4.88 J/cm² Grade Count:13 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Charpy Impact Unnotched | 2.70 J/cm² | 12.8 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |