Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.00 - 1.30 J/cm² | 4.76 - 6.19 ft-lb/in² | ISO 11542-2 |
Okulen® 1000 PE-UHMW, AST OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 - REG PE Colored OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 1.50 J/cm² | 4.76 - 7.14 ft-lb/in² | ISO 11542-2 |
Okulen® 500 - REG PE Multicoloured fine OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne Edgetek® QT-20MN/000 natural HI Syndiotactic Polystyrene (SPS) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 1.00 - 1.90 J/cm² | 4.76 - 9.04 ft-lb/in² | Average value: 1.48 J/cm² Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 678C Polystyrene
(discontinued **) STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
Polimeri Europa EDISTIR N1671 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol.. |
|||
Charpy Impact Unnotched | 1.00 - 1.20 J/cm² @Temperature 23.0 °C |
4.76 - 5.71 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² - NB | 4.76 ft-lb/in² - NB | Average value: 3.77 J/cm² Grade Count:30 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed
&nbs Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Laramid CE/60 PPA, 60% Mineral Reinforced Semi-aromatic polyamide (PPA) based compound. Mineral filler. High dimensional stability. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latimass 75/4-04 D009 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latishield 36/AR-10A-V0E ABS, Steel Fiber Reinforced, Flame Retardant EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Information provided by Lati Indust.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latistat 36/MR-04 ABS Dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179 |
Styrolution PS 124 N/L GPPS Styrolution PS 124N/L is a general purpose polystyrene grade with a good flow characteristic and an improved heat resistance.Excellent flow propertiesHigh heat resistanceUL 94 HB (Antwerp only)Infor.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179 |
Styrolution PS 485N HIPS Styrolution PS 485N is a high impact grade of polystyrene for extruded sheets with a matte surface.Matte SurfaceUL 94 HBInformation provided by Styrolution |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9331 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers, indicator and brake light lenses.Information provided by Bayer.As of 1 September 2015, Ba.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Dow Tyril® 990 SAN TYRIL® 990 SAN copolymer grade provides colorless glass-like clarity and excellent overall optical properties. It provides a profile of very good strength with stiffness, chemical resistance, heat .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data |
Dow Tyril® 1000B SAN TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® C40H 455 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® C40H 458 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1189 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.00 - 1.50 J/cm² | 4.76 - 7.14 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² - NB @Temperature -30.0 - -30.0 °C |
4.76 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 2.19 J/cm² Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² - NB | 4.76 ft-lb/in² - NB | Average value: 3.90 J/cm² Grade Count:21 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Charpy Impact Unnotched | 1.00 - 4.70 J/cm² @Temperature -20.0 - -20.0 °C |
4.76 - 22.4 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 2.98 J/cm² Grade Count:4 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |