Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded
Manufacturer Dow Chemical
Trade Name Tyril®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Tyril® 125 SAN.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM Data
Melt Density 0.914 g/cc
0.0330 lb/in³
Melt density
Melt Flow 25 g/10 min

@Load 3.80 kg,
Temperature 230 °C
25 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ASTM Data
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM Data
Elongation at Break 1.5 %
1.5 %
ASTM Data
Tensile Modulus 3.31 GPa
480 ksi
ASTM Data
Charpy Impact Unnotched 1.00 J/cm²
4.76 ft-lb/in²
ISO Data
1.00 J/cm²
4.76 ft-lb/in²
ISO Data, Low Temp
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
ISO Data, Low Temp
0.200 J/cm²
0.952 ft-lb/in²
ISO Data
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature 20.0 °C
35.0 µin/in-°F

@Temperature 68.0 °F
ISO data
Specific Heat Capacity 1.68 J/g-°C
0.402 BTU/lb-°F
Thermal Conductivity 0.113 W/m-K
0.784 BTU-in/hr-ft²-°F
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Unannealed; ASTM Data
Vicat Softening Point 113 °C
235 °F
Optical Properties Metric English Comments
Haze 0.45 %
0.45 %
Transmission, Visible 91 %
91 %