Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers PC/PBT-1230 Polycarbonate+PBT, General Purpose, Injection Grade

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Lucent Polymers PC/PBT-1230 Polycarbonate+PBT, General Purpose, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
1/8" Section
Melt Flow 30 g/10 min

@Load 5.00 kg,
Temperature 260 °C
30 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Elongation at Break >= 118 %
>= 118 %
ASTM D638
Flexural Strength 84.83 MPa
12300 psi
ASTM D790
Flexural Modulus 2.034 GPa
295.1 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 101.67 °C
215.01 °F
ASTM D648