Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML4351 PC (Asia Pacific) |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
9.18 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880... |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.20 mm |
9.18 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 4.90 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 9.18 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP1007FE Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333HI5BL High Impact Nylon 66 Middle viscosity, Impact -resistantApplications A variety of fuse boxes, relax boxesInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
Global B-5200 High Density Polyethylene Description-has excellent stiffness thus requires less material to make
blow moldingApplications-food containers, drinking bottles, medicine bottles, water containersInformation provided by Global .. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
Global B-8200 High Density Polyethylene Description-high molecular weight, excellent stress cracking resistance,
excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi.. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
Global F-8000 High Density Polyethylene Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | >= 4.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 9.18 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 4.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 9.18 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
9.18 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 4.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 9.18 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 4.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 9.18 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY ER5001RF PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (All in One PC & Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by .. |
|||
Izod Impact, Notched | >= 4.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 9.18 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.17 mm |
9.18 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.17 mm |
9.18 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.17 mm |
9.18 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.17 mm |
9.18 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.17 mm |
9.18 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.90 J/cm @Thickness 3.17 mm |
9.18 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.90 J/cm @Temperature -10.0 °C |
9.18 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LX2801 PC (Asia Pacific) |
|||
Izod Impact, Notched | 4.90 J/cm | 9.18 ft-lb/in | ASTM D256 |
SK Chemicals SKYPEL P155D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |