Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 4.90 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® ML4351 PC (Asia Pacific)
Izod Impact, Notched 4.90 J/cm
<br>@Thickness 3.18 mm,<br> Temperature 23.0 °C
9.18 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
Compression Molded; ASTM D256A
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880...
Izod Impact, Notched 4.90 J/cm
<br>@Thickness 3.20 mm
9.18 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
LG Chemical AP163 ABS, Permanent Anti-Static
Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched >= 4.90 J/cm
<br>@Thickness 6.40 mm,<br> Temperature 23.0 °C
>= 9.18 ft-lb/in
<br>@Thickness 0.252 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Kolon KOPA® KN333HI5BL High Impact Nylon 66
Middle viscosity, Impact -resistantApplications A variety of fuse boxes, relax boxesInformation provided by API-Kolon.
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Global B-5200 High Density Polyethylene
Description-has excellent stiffness thus requires less material to make blow moldingApplications-food containers, drinking bottles, medicine bottles, water containersInformation provided by Global ..
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Global B-8200 High Density Polyethylene
Description-high molecular weight, excellent stress cracking resistance, excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi..
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Global F-8000 High Density Polyethylene
Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation.
Izod Impact, Notched >= 4.90 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
>= 9.18 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY EC5000A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical
Izod Impact, Notched >= 4.90 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
>= 9.18 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence
Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical
Izod Impact, Notched >= 4.90 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
>= 9.18 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY EF5001RFT PC/ABS
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical..
Izod Impact, Notched 4.90 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
9.18 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Izod Impact, Notched >= 4.90 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
>= 9.18 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY MP5000AM PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Izod Impact, Notched >= 4.90 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
>= 9.18 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY ER5001RF PC/ABS
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (All in One PC & Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by ..
Izod Impact, Notched >= 4.90 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
>= 9.18 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ357 PBT+PC
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Izod Impact, Notched 4.90 J/cm
<br>@Thickness 3.17 mm
9.18 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.90 J/cm
<br>@Thickness 3.17 mm
9.18 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.90 J/cm
<br>@Thickness 3.17 mm
9.18 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.90 J/cm
<br>@Thickness 3.17 mm
9.18 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SK Chemicals SKYPEL P147D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Izod Impact, Notched 4.90 J/cm
<br>@Thickness 3.17 mm
9.18 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.90 J/cm
<br>@Temperature -10.0 °C
9.18 ft-lb/in
<br>@Temperature 14.0 °F
ASTM D256
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LX2801 PC (Asia Pacific)
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
SK Chemicals SKYPEL P155D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..