Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.850 J/cm @Temperature -40.0 °C |
1.59 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycolac® X11 ABS Automotive: High heat resistance. Excellent flow/impact balance. UL94 HB rated. High gloss. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM4219 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Asia Pacific) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched | 0.849 - 5340 J/cm | 1.59 - 10000 ft-lb/in | Average value: 3.88 J/cm Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC PP 674K Polypropylene Copolymer for Injection Molding Product Description: PP 674K is specially developed for producing injection molded & ISBM articles with high clarity and also has better impact properties than homo PP counterparts.PP 674K has the .. |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA66-G15 15% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lavergne VYPET VNT 615 PET 15% Glass Reinforced Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 553 PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 0.000 °C |
1.59 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SPS Guang Zhou POLLITEâ„¢ 1002G30 Flame-retarded/GF30%-Polycarbonate Characteristic: High mechanical properties, high rigidity, high heat resistant, good dimensional stability, good flame retardanceApplications: E/E parts, power tool, office suppliesInformation Provi.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA (Asia Pacific) LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber 30% glass fiber reinforced, high thermal resistance high UV and radiation PVDF for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM-D256 |
Braskem IA59U3 HDPE Injection Molding Polyethylene Homopolymer IA59U3 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high stiffness and impact strength combined .. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-200NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low mainten.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |