Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. Available in limited colors.
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Density 1.53 g/cc
0.0553 lb/in³
ISO 1183
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0600 %
0.0600 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.26 %
0.26 %
ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 1.50 - 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.0591 - 0.126 in
SABIC Method
0.0030 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
0.0050 - 0.0080 cm/cm

@Thickness 3.20 - 4.60 mm
0.0050 - 0.0080 in/in

@Thickness 0.126 - 0.181 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Thickness 1.50 - 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.0591 - 0.126 in
SABIC Method
0.0060 - 0.0090 cm/cm

@Thickness 3.20 - 4.60 mm
0.0060 - 0.0090 in/in

@Thickness 0.126 - 0.181 in
SABIC Method
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 250 °C
26 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 250 °C
20 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 120 MPa
17400 psi
Type I, 5 mm/min; ASTM D638
125 MPa
18100 psi
5 mm/min; ISO 527
Tensile Strength, Yield 120 MPa
17400 psi
Type I, 5 mm/min; ASTM D638
125 MPa
18100 psi
5 mm/min; ISO 527
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
3.0 %
3.0 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 2.0 %
2.0 %
5 mm/min; ISO 527
3.0 %
3.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 9.30 GPa
1350 ksi
5 mm/min; ASTM D638
9.30 GPa
1350 ksi
1 mm/min; ISO 527
Flexural Strength 189 MPa
27400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 195 MPa
28300 psi
2 mm/min; ISO 178
Flexural Modulus 7.58 GPa
1100 ksi
1.3 mm/min, 50 mm span; ASTM D790
8.50 GPa
1230 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
0.800 J/cm

@Temperature -30.0 °C
1.50 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 8.01 J/cm
15.0 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
25.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
25.2 µm/m-°C

@Temperature 60.0 - 138 °C
14.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature -40.0 - 40.0 °C
66.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 215 °C

@Thickness 6.40 mm
419 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
207 °C

@Thickness 6.40 mm
405 °F

@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 215 °C
419 °F
Rate B/50; ASTM D1525
215 °C
419 °F
Rate B/50; ISO 306
220 °C
428 °F
Rate B/120; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity >= 3.20e+16 ohm-cm
>= 3.20e+16 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
ASTM D150
3.8

@Frequency 100 Hz
3.8

@Frequency 100 Hz
ASTM D150
Dielectric Strength 18.7 kV/mm

@Thickness 3.20 mm
475 kV/in

@Thickness 0.126 in
in air; ASTM D149
24.8 kV/mm

@Thickness 1.60 mm
630 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor 0.0020

@Frequency 100 Hz
0.0020

@Frequency 100 Hz
ASTM D150
0.020

@Frequency 1.00e+6 Hz
0.020

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Specific Volume 0.65 cm^3/g
ASTM D792
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved