Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC5210 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Rotuba MS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 6.35 mm |
1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection
(discontinued **)& Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.690 - 6.57 J/cm | 1.29 - 12.3 ft-lb/in | Average value: 4.11 J/cm Grade Count:5 |
Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products
(discontinued **) ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and .. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Udel® P-1835 Polysulfone (PSU)
(discontinued **) Udel P-1835 polysulfone is a powdered grade well suited for the fabrication of porous membranes. The membranes can be made into hollow fibers, tubes, plates, or spiral wound elements. They are used .. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN1322VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.686 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 1.29 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP2200 PP+GF20% Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN333HS Heat Resistant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific) 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-pro.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EC002XXQ PEI LNP* THERMOCOMP* EC002XXQ is a compound based on Polyetherimide containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp MF006ASJ PP LNP THERMOCOMP* MF006ASJ is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized, Healthcare.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EM7301F PPE+PS 10% glass-reinforced. HDT 252F. Good flow and polyurethane foam adhesion. Black only. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | |
UBE UBEPOL BR34HL HIPS (stirring rate = 500 rpm) Description: UBEPOL-BR34HL is characterized by its lower molecular weight and higher linear molecular chain compared with UBEPOL-BR15HB. The properties of HIPS modified by UBEPOL-BR34HL are very goo.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T888G15 PBT, 15% Glass Fiber |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 714 PPS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | Conditioned; ASTM D256 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |