| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
| 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.850 % | 0.850 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0135 cm/cm <br>@Time 86400 sec |
0.0135 in/in <br>@Time 24.0 hour |
ISO 294 |
| 0.014 cm/cm <br>@Time 86400 sec |
0.014 in/in <br>@Time 24.0 hour |
ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm <br>@Time 86400 sec |
0.013 in/in <br>@Time 24.0 hour |
ASTM D955 |
| 0.0133 cm/cm <br>@Time 86400 sec |
0.0133 in/in <br>@Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 7.00 MPa | 1020 psi | ISO 527 |
| 18.0 MPa | 2610 psi | ASTM D638 | |
| Tensile Strength, Yield | 28.0 MPa | 4060 psi | ASTM D638 |
| 28.0 MPa | 4060 psi | ISO 527 | |
| Elongation at Break | 47 % | 47 % | ASTM D638 |
| 98.2 % | 98.2 % | ISO 527 | |
| Elongation at Yield | 8.0 % | 8.0 % | ISO 527 |
| 9.6 % | 9.6 % | ASTM D638 | |
| Tensile Modulus | 1.35 GPa | 196 ksi | 1 mm/min; ISO 527 |
| 1.39 GPa | 202 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 32.0 MPa | 4640 psi | ISO 178 |
| 40.0 MPa | 5800 psi | ASTM D790 | |
| Flexural Modulus | 1.36 GPa | 197 ksi | ISO 178 |
| 1.44 GPa | 209 ksi | ASTM D790 | |
| Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 7.00 J | 5.16 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 5.00 J | 3.69 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 110 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 110 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 128 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
71.1 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 128 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
71.1 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 100 °C <br>@Thickness 3.20 mm |
212 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 59.0 °C | 138 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 56.0 °C <br>@Thickness 3.20 mm |
133 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |