Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
PolyMirae Moplen EP540S Injection Molding Grade Polypropylene Moplen EP540S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540S is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
PolyMirae Moplen EP540T Injection Molding Grade Polypropylene Moplen EP540T is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540T is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® SG5152 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good Surface, High ImpactApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG.. |
|||
Izod Impact, Notched | 0.686 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 .. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN133HR Heat Resistant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN133MT40 M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN135HB40SIBL Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN3311N General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN331F General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2306FY PBT+GF30% Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided .. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUSEP SP2306F SPS+GF30%, Flame Retardant Feature: Injection Molding, sPS+GF30%, Flame RetardantApplication: Pump Units, Pick-up Lends Holder, etcCAS No. 9003-53-6, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | |
Shinil Chemical SHINCON PES-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | |
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Window Strip SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N66C3 Nylon 66, 30% Mineral Reinforced |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T882GV15 Flame Retardant PBT, 15% Glass Fiber |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T888G15 PBT, 15% Glass Fiber |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV3050 Polyformaldehyde |
|||
Izod Impact, Notched | >= 0.686 J/cm @Thickness 6.35 mm |
>= 1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP213G15 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH50GM 30% Glass Fiber Reinforced Mineral Filled Low Warpage Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |