Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.510 J/cm @Thickness 3.18 mm, Temperature -40.0 °C |
0.955 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.510 J/cm @Temperature 23.0 °C |
0.955 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AS33L-07VS Polypropylene, Rubber modified, Compounded Description: AS33L-07 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key.. |
|||
Izod Impact, Notched | 0.510 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.955 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy) Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold.. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22I PA 66 LNP* LUBRICOMP* RAL22I is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant, High Impact. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66 LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Izod Impact, Notched | 0.510 J/cm @Temperature -30.0 °C |
0.955 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s). |
|||
Izod Impact, Notched | 0.510 J/cm @Temperature 23.0 °C |
0.955 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |
|||
Izod Impact, Notched | 0.510 J/cm @Temperature -40.0 °C |
0.955 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
Styrolution Luran® S 776 SE ASA Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between .. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF006AS PP LNP THERMOCOMP* MF006AS is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | |
UBE C (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBE high impact polystyrene (HIPS).Information provided by UBE. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
Cheng Yu Plastic PP236G1 Polypropylene, 10% Glass Fiber |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Izod Impact, Notched | 0.510 J/cm | 0.955 ft-lb/in | ASTM D256 |
Plenco 50335 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |