Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.440 J/cm @Temperature -30.0 °C |
0.824 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Gharda Chemicals GATONE™ 5700 Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Izod Impact, Notched | 0.440 - 0.961 J/cm | 0.824 - 1.80 ft-lb/in | Average value: 0.714 J/cm Grade Count:13 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.440 - 3.20 J/cm @Temperature -50.0 - 0.000 °C |
0.824 - 5.99 ft-lb/in @Temperature -58.0 - 32.0 °F |
Average value: 1.44 J/cm Grade Count:19 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
LNP ULTEM® JD7107 Polyetherimide
(discontinued **) Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® GF305 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® GF705 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffnessApplications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® K300BK Black Colored Grade Acetal Resin Colored, general purpose injection molding grade. Applications: General injection molding products.Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® K300HRD Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® MS301 Wear Modified Acetal Resin Molybdenum disulfide added, improved wear property. Applications: Products for low noise and friction against metal. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® SO301 Wear Modified Acetal Resin Silicone Oil added, improved wear property. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® WR301 Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Kolon KOCETAL® WR301LO Wear Modified Acetal Resin Improved weather resistance and low odor of FA. Applications: Weather resistant products at closed space. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66 LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM JD7101 PEI (Asia Pacific) |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Izod Impact, Notched | 0.440 J/cm @Temperature 23.0 °C |
0.824 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP JF003E PES LNP* THERMOCOMP* JF003E is a compound based on Polyethersulfone resin containing 15% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX06420 PA 66 LNP* Thermocomp* RX06420 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Low Extractible, Mold Release. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Plenco 6015 Phenolic, Briquette, Transfer Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Plenco 6401 Phenolic, Briquette, Transfer Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Izod Impact, Notched | 0.440 J/cm | 0.824 ft-lb/in | ASTM D256 |
Unitika M2350 PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.440 J/cm @Thickness 3.17 mm |
0.824 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.440 J/cm @Temperature -20.0 °C |
0.824 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Total PPC 4824WZ Polypropylene, Impact Copolymer ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent .. |
|||
Izod Impact, Notched | 0.440 - 0.480 J/cm | 0.824 - 0.899 ft-lb/in | ASTM D256A |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |
|||
Izod Impact, Notched | 0.440 - 0.540 J/cm @Thickness 6.35 mm |
0.824 - 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT1200M General Purpose PBT Information provided by Dowell Trading Company Ltd. |