Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LNP ULTEM® JD7107 Polyetherimide  (discontinued **)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LNP ULTEM® JD7107 Polyetherimide  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 128 MPa
18600 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 5.09 GPa
738 ksi
ASTM D790
Izod Impact, Notched 0.440 J/cm
0.824 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 10000 - 1.00e+6 ohm
10000 - 1.00e+6 ohm
ASTM D257