Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.270 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.506 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ FR PP 301 S Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Izod Impact, Notched | 0.270 - 8.17 J/cm | 0.506 - 15.3 ft-lb/in | Average value: 1.31 J/cm Grade Count:11 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
Ineos Nova Zylar® 220 High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent moldability, High clarity, Extended toughness and elongation, meets USP XXI specification for Class VI Plastics, Property retention after gamma irradiationApplications: Display, medical de.. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature 23.0 °C |
0.506 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol H200MA Polypropylene REPOL Polypropylene H200MA is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256A |
DSM Somos® 7120 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Izod Impact, Notched | 0.270 - 1.33 J/cm | 0.506 - 2.50 ft-lb/in | Average value: 0.776 J/cm Grade Count:80 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
Flint Hills P5C6Z-075 Random Copolymer Polypropylene Features: Phthalate-free.Applications: Fibers, BCF, SpunbondedInformation provided by Flint Hills Resources. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material .. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + .. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature 23.0 °C |
0.506 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon IS000LX PA6.12 LNP* Stat-Kon* IS000LX is a compound based on Nylon 6/12 containing Stainless Steel Fibers.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -30.0 °C |
0.506 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PX1736 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | |
Cosmic Plastics E4920 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar GN071 Natural PETG Copolyester EASTAR GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions wi.. |
|||
Izod Impact, Notched | 0.270 J/cm @Thickness 3.17 mm |
0.506 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PP-HP20 Homopolymer, 20 Melt Flow This product can be used for general purpose injection molding as well as fiber spinning and other critical extrusion applicationsInformation provided by Entec |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 93A Nanoclay Cloisite® 93A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D-785 |
Bapolene® 4017 Polypropylene Bapolene 4017 is a homopolymer polypropylene with outstanding modulus. It complies with FDA 21 CFR1777.1520.Applications: Strapping, profile extrusion, and general purpose.Bapolene® and Bapolan® .. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
Bapolene® 4052F Polypropylene, Blown Film Grade Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FD.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 631 Nylon 6/6, Glass Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
Plenco 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 302 is a two-stage, woodflour and flock-filled phenolic molding compound. It has low specific gravity, broad molding latitude and an excellent balance of electrical and physical properties... |
|||
Izod Impact, Notched | 0.270 - 1.07 J/cm | 0.506 - 2.00 ft-lb/in | Average value: 0.616 J/cm Grade Count:41 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America TEM 9053C Hardware Grade Epoxy Short fiberglass and mineral filled, toughened epoxy molding compound with excellent dimensional stability and high strength properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256A |
LyondellBasell Astryn 65F5-4 Polypropylene Homopolymer, 40% Calcium Carbonate Key Features: conventional melt flow, high modulus, mineral-filled polypropylene homopolymer, high stiffness, excellent chemical resistance, good surface qualityApplications: automotive components, .. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 663 Nylon 6, Glass Bead Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has .. |