Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Nylene® 406 Nylon 6, 50% RH Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have bet.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Nylene® 406F Nylon 6, 50% RH Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin.
.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Nylene® 409 Nylon 6, 50% RH Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Izod Impact, Notched | >= 2.50 J/cm | >= 4.68 ft-lb/in | blow molding |
Reliance Industries Polypropylene Impact Copolymer Typical properties of Reliance - Repol Polypropylene grades. Properties depend on rubber content, presence of nucleating agent, MFIInformation provided by Reliance Industries |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -40.0 °C |
4.68 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Covestro Bayblend® 2753 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.17 mm |
4.68 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Hannam Chemical Hanalac 780 ABS, High Flow FDA Approved. High flow grade suitable for intricate or thin structures and low processing cycle time. Applications include TVs, radios, calculators, appliances, toys. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | BS 2782.306A |
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -20.0 °C |
4.68 ft-lb/in @Temperature -4.00 °F |
BS 2782.306A |
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
4.68 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.17 mm |
4.68 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Hannam Chemical Hanalac 750 ABS, General Purpose FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: elect.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -20.0 °C |
4.68 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS (Asia Pacific) Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Styrolution Luran® S 778 Q42 Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.17 mm |
4.68 ft-lb/in @Thickness 0.125 in |
ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Styrolution Luran® S 778 UV Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 (Asia Pacific) LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder, Impact Modifier. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D256 |
Unitika M1030B PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA844 Nylon 6.6, UV Stabilized Impact modified, UV and heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P50N01 Homopolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PV507 ABS, Flame Retardant Flame retardant ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.50 J/cm | 4.68 ft-lb/in | |
Bapolan® ABS8430 ABS Polymer, Extrusion/Injection Grade Applications: Electronic Instruments, appliances.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.68 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® A0210 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |