Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific) Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.39 ft-lb/in | ASTM D256 |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.39 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN133G33SIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm |
2.39 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co.. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature 23.0 °C |
2.38 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® SM340 Polypropylene impact copolymer Titanpro® SM340 is an intermediate impact material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adju.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature 23.0 °C |
2.38 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12 LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm |
2.39 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TX-0510T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm |
2.39 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trimma® SD6310H PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific) LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10 LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature -30.0 °C |
2.38 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN3L PPE+HIPS (Asia Pacific) PPE+PS, GF30%, hydrolytic stability improved |
|||
Izod Impact, Notched | 1.27 J/cm | 2.39 ft-lb/in | ASTM D256 |
Cheng Yu Plastic ML3435 PC, 35% Glass Fiber |
|||
Izod Impact, Notched | 1.27 J/cm | 2.39 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T890G3 PBT, 30% Glass Fiber |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 13G43 43% Glass Filled Nylon 66 43% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Mechanical and electrical parts such as micromotors, automotive parts such as radiator tanks and shift leversInformation provi.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 90G50 50% Glass Filled Nylon 66 Enhanced strength and stiffness; with 50% GF. Excellent appearance.Applications:Office furnitureInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G8-43GF Nylon 66, 43% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.39 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® V250A 50% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.39 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH50G3 30% Glass Fiber Reinforced High Strength Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Izod Impact, Notched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |