Material Notes:
LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact performance, Non-Brominated & Non-Chlorinated Flame Retardant.
Physical Properties Metric English Comments
Density 1.635 g/cc
0.05907 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cm
<br>@Time 86400 sec
0.00050 - 0.0020 in/in
<br>@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.00050 - 0.0020 cm/cm
<br>@Time 86400 sec
0.00050 - 0.0020 in/in
<br>@Time 24.0 hour
ASTM D955
Melt Flow 13 g/10 min
<br>@Load 2.16 kg,<br> Temperature 300 °C
13 g/10 min
<br>@Load 4.76 lb,<br> Temperature 572 °F
ASTM D1238
48.6 g/10 min
<br>@Load 5.00 kg,<br> Temperature 300 °C
48.6 g/10 min
<br>@Load 11.0 lb,<br> Temperature 572 °F
ASTM D1238
Melt Index of Compound 29 g/10 min
<br>@Load 5.00 kg,<br> Temperature 300 °C
29 g/10 min
<br>@Load 11.0 lb,<br> Temperature 572 °F
MVR [cm^3/10 min]; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 153 MPa
22200 psi
5 mm/min; ISO 527
154 MPa
22300 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.9 %
1.9 %
5 mm/min; ISO 527
2.1 %
2.1 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 15.13 GPa
2194 ksi
1 mm/min; ISO 527
15.32 GPa
2222 ksi
5 mm/min; ASTM D638
Flexural Strength 223 MPa
32300 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 14.87 GPa
2157 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.27 J/cm
2.38 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.20 J/cm
9.74 ft-lb/in
ASTM D4812
Charpy Impact Unnotched 3.80 J/cm²
18.1 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
<br>@Thickness 3.20 mm
225 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0
<br>@Thickness 1.00 mm
V-0
<br>@Thickness 0.0394 in
UL 94