Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.880 J/cm @Temperature -40.0 °C |
1.65 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature -30.0 °C |
1.65 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature -30.0 °C |
1.65 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature -30.0 °C |
1.65 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
Reliance Industries Relene M60075 Polyethylene Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade.. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LGN2000 PC (Asia Pacific) |
|||
Izod Impact, Notched | 0.880 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARPEEK 50 G/60 60% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
Reliance Industries Relene L60075 Polyethylene Relene L60075 is UV stabilized. It is available with a recommended service life of more then 5 years L60075 is suitable for applications where articles are exposed to sunlight e.g. soft drink crates.. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SP7602 PC (Asia Pacific) |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66 EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-5306F General Purpose PC/ABS Alloy, 30% Polymer Alloy, Weather Resistant, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL S100G10 PPE+PS (Asia Pacific) |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL S100G20 PPE+PS (Asia Pacific) |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 507 PBT+PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® VC120 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7602 PC (Asia Pacific) |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump.. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GFN2L PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX880 PPE+PA6 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HFG300 PPE+PS (Asia Pacific) PPE+PS GF30% filled, FR V-0 |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL LEN2231 PPE+HIPS (Asia Pacific) PPE+PS Unfilled for LED Application |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GN390 PPE+PS (Asia Pacific) Closed loop recycle grade for CANON, 13% PCR-PS loaded, HDT 90C, V-0/1.2mm |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX APS130 PPE+PPS (Asia Pacific) PPE+PPS GF30% |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX6801 PPE+PA (Asia Pacific) PPE+PA, GF 30% |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX6801 PPE+PS+PA66 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE. |
|||
Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL APS130 PPE+PPS (Asia Pacific) |