SABIC Innovative Plastics Noryl GTX GTX6801 PPE+PS+PA66 (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl GTX GTX6801 PPE+PS+PA66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D 792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 142 MPa
20600 psi
SABIC - Japan Method
Elongation at Break 10 %
10 %
SABIC - Japan Method
Flexural Strength 215 MPa
31200 psi
ASTM D 790
Flexural Modulus 8.43 GPa
1220 ksi
ASTM D 790
Izod Impact, Notched 0.880 J/cm

@Temperature 23.0 °C
1.65 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 30.0 - 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 230 °C

@Thickness 3.20 mm
446 °F

@Thickness 0.126 in
unannealed; ASTM D 648