SABIC Innovative Plastics NORYL LEN2231 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics NORYL LEN2231 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PPE+PS Unfilled for LED Application
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 4.6 g/10 min

@Load 10.0 kg,
Temperature 250 °C
4.6 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 59.0 MPa
8560 psi
SABIC - Japan Method
Elongation at Break 40 %
40 %
SABIC - Japan Method
Izod Impact, Notched 0.880 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 122 °C

@Thickness 6.40 mm
252 °F

@Thickness 0.252 in
unannealed; ASTM D648