Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Plaskolite Duraplex® 50% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2EU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Izod Impact, Notched | 0.700 - 1.10 J/cm @Temperature -40.0 - 0.000 °C |
1.31 - 2.06 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.945 J/cm Grade Count:2 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | Molded; ASTM D256 |
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256A |
LyondellBasell Pro-fax SB891 Polypropylene Impact Copolymer Key Features: high flow, compatible with hindered amine light stabilizers, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling and minimum warpageAppli.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2200F PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -40.0 °C |
1.31 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Sterigenics Raprex® R100D Branched High Density Polyethylene Applications: ExtrusionRAPREX® R100D is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched struct.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific) LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm |
1.31 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP6432 9690 Medium Impact Polystyrene Characteristics High flow Good toughness Available in various colors Processing Injection moldingApplications Air conditioner and cooler grills Refrigerator parts Washing machine components Mate.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, flame retardant, halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ISO 180 |
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM7009 Acetal, UV Stabilized UV stabilized polyacetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Unitika M1030E PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiter PBT GF 20 Polybutylene Terephthalate, 20% Glass Characteristics: 20% glass fibre filled |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.700 - 1.30 J/cm @Thickness 6.35 mm |
1.31 - 2.44 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |