Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792, ISO 1183 |
Water Absorption | 0.30 % @Temperature 23.0 °C |
0.30 % @Temperature 73.4 °F |
24h; ASTM D570, ISO 62 |
Linear Mold Shrinkage | 0.0025 - 0.015 cm/cm | 0.0025 - 0.015 in/in | ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 83 | 83 | ASTM D785, ISO 2039/2 |
Tensile Strength, Yield | 118 MPa | 17100 psi | ASTM D638, ISO R527 |
Elongation at Break | 3.0 % | 3.0 % | ASTM D638, ISO R527 |
Flexural Strength | 185 MPa | 26800 psi | ASTM D790, ISO 178 |
Flexural Modulus | 6.30 GPa | 914 ksi | ASTM D790, ISO 178 |
Izod Impact, Notched | 0.700 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 140 °C | 284 °F | 20000 h; VDE 0304/P2-1, IEC 216 |
160 °C | 320 °F | 5000 h; VDE 0304/P2-1, IEC 216 | |
200 °C | 392 °F | few hours; VDE 0304/P2-1, IEC 216 | |
Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | ASTM D648, ISO 75 |
Vicat Softening Point | 210 °C @Load 5.00 kg |
410 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
220 °C @Load 0.999 kg |
428 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A | |
Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
|
HB @Thickness 3.20 mm |
HB @Thickness 0.126 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257, IEC 93 |
Dielectric Constant | 3.8 @Frequency 1000 Hz |
3.8 @Frequency 1000 Hz |
ASTM D150, IEC 250 |
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149, IEC 243 |
Dissipation Factor | 0.0020 @Frequency 1000 Hz |
0.0020 @Frequency 1000 Hz |
ASTM D150, IEC 250 |
Comparative Tracking Index | 400 V | 400 V | VDE 0303-P1, IEC 112 |