Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
PolyMirae Moplen 341R Injection Molding Grade Polypropylene Moplen RP341R is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP341R is a random copolymer particularly suitable for injecti.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
PolyMirae Moplen HF524J BDDP Film Grade Polypropylene Moplen HF524J is the Addiform polypropylene. Compared to ordinary pelletized polypropylene, Addiform gives significant advantages in terms of improved productivity, better processing and lower energ.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP513FLBL Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 0.918 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCON PS4200 ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 23.0 mm, Temperature 3.20 °C |
0.918 ft-lb/in @Thickness 0.906 in, Temperature 37.8 °F |
ASTM D256 |
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP2100 PP+GF10% Description: Injection Molding, PP+GF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Kolon KOPA® KN3322V0Y Flame Retardant Nylon 66 Halogen free, Impact -resistantApplications A variety of connectorsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC R3400 Polypropylene Random Copolymer Features: Seetec R3400 is a polypropylene-ethylene random copolymer designed for non-transparent injection molding application. SEETEC R3400 meets the FDA requirement in the code of Federal Regulati.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® 6531M Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 2564PCX TA6 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTH CONTAIN UV STABILIZER AND LONG TERM HEAT AGING ADDITIVESAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, .. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
|
Kuraray SEPTON® CM1 Compatibilizer Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem JD7902 PEI (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | |
Shinil Chemical SHINSTAT PC Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® EM-8240C MPPE, Glass Filled MPPE/GF material that is used in the main frame of banknote sortersInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tramid® 910 PA66/PA6 Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.Applications:Automotive knob types, door handles and mirror housingsConnectorsCab.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NC212 PPE+HIPS (Asia Pacific) |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika UG-100-20 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | |
Zylog Hipolyene® 8515 TY Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N66C1 Nylon 66, 10% Mineral Reinforced |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Daelim H&L Plavis-G15 ISO 15% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded .. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G2-13GF Nylon 66, 13% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm |
0.918 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm |
0.918 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Izod Impact, Notched | 0.490 - 1.82 J/cm | 0.919 - 3.40 ft-lb/in | Average value: 0.880 J/cm Grade Count:45 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |