Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.470 J/cm @Temperature 23.0 °C |
0.881 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARPEEK 10 K/20 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
Kolon KOCETAL® CF702 Conductive Grade Acetal Resin Carbon fiber added, high stiffness and conductive grade. Applications: Conductive products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP PL002 PA 6 LNP* LUBRICOMP* PL002 is a compound based on Nylon 6 base resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66 LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE0049F PC LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding... |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Izod Impact, Notched | 0.470 J/cm @Temperature 0.000 °C |
0.881 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Izod Impact, Notched | 0.470 J/cm @Temperature -30.0 °C |
0.881 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON OE004AE PPS - Branched LNP STAT-KON* OE004AE is a compound based on PPS - Branched resin containing 20% Carbon Fiber. Added features of this material are: Easy Molding, Electrically Conductive. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.880 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l.. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
Plenco 6582 Phenolic, Briquette, Transfer Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Izod Impact, Notched | 0.470 J/cm @Thickness 3.17 mm |
0.881 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika LM-8503-10 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
Unitika RUN35-C25 Weather resistant PA6, Dry Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.470 - 0.520 J/cm | 0.881 - 0.974 ft-lb/in | ASTM D256A |
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features.. |
|||
Izod Impact, Notched | 0.470 J/cm | 0.880 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336C30L1 Calcium Reinforced |
|||
Izod Impact, Notched | 0.470 J/cm | 0.880 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339G15M15CL Glass/Mineral Reinforced Coupled |