Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Carbon Fiber Filled
Manufacturer Kolon
Trade Name Kocetal®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOCETAL® CF702 Conductive Grade Acetal Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Carbon fiber added, high stiffness and conductive grade. Applications: Conductive products. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.22 %
0.22 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 87
87
ASTM D785
Tensile Strength 80.0 MPa
11600 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 6.60 GPa
957 ksi
ASTM D790
Izod Impact, Notched 0.470 J/cm
0.881 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C
33.3 µin/in-°F
ASTM D696
Melting Point 166 °C
331 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
327 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Surface Resistance 1.00e+7 ohm
1.00e+7 ohm
ASTM D257