DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer
Manufacturer DSM Somos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features. Applications include short run manufacturing, functional end use performance prototypes such as snap-fit designs, impellers, duct work, connectors, electronic covers, automotive housings, dashboard assemblies, packaging and sporting goods.Property data for post-cured polymer.Information provided by Axis Prototypes.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Liquid
Water Absorption 0.39 - 0.41 %
0.39 - 0.41 %
ASTM D570-98
Viscosity 1000 cP

@Temperature 30.0 °C
1000 cP

@Temperature 86.0 °F
Liquid
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
ASTM D2240
Tensile Strength at Break 31.0 - 34.6 MPa
4500 - 5020 psi
ASTM D638M
Tensile Strength, Yield 41.1 - 43.3 MPa
5960 - 6280 psi
ASTM D638M
Elongation at Break 8.0 - 10 %
8.0 - 10 %
ASTM D638M
Elongation at Yield 3.0 %
3.0 %
ASTM D638M
Tensile Modulus 2.37 - 2.49 GPa
344 - 361 ksi
ASTM D638M
Flexural Strength 67.8 - 70.8 MPa
9830 - 10300 psi
ASTM D790M
Flexural Modulus 2.415 - 2.525 GPa
350.3 - 366.2 ksi
ASTM D790M
Poissons Ratio 0.42 - 0.44
0.42 - 0.44
ASTM D638M
Shear Modulus 0.875 GPa
127 ksi
calculated
Izod Impact, Notched 0.470 - 0.520 J/cm
0.881 - 0.974 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear 71.5 - 74.3 µm/m-°C

@Temperature -40.0 - 0.000 °C
39.7 - 41.3 µin/in-°F

@Temperature -40.0 - 32.0 °F
ASTM E831-05
106.5 - 114.5 µm/m-°C

@Temperature 0.000 - 50.0 °C
59.17 - 63.61 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-05
168.6 - 175.4 µm/m-°C

@Temperature 50.0 - 100 °C
93.67 - 97.44 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-05
168.8 - 176.4 µm/m-°C

@Temperature 100 - 150 °C
93.78 - 98.00 µin/in-°F

@Temperature 212 - 302 °F
ASTM E831-05
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 57.0 °C
131 - 135 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 51.0 °C
118 - 124 °F
ASTM D648
Glass Transition Temp, Tg 43.0 - 47.0 °C
109 - 117 °F
ASTM E1545-00
Electrical Properties Metric English Comments
Dielectric Constant 3.62

@Frequency 1.00e+6 Hz
3.62

@Frequency 1.00e+6 Hz
ASTM D150-98
3.97

@Frequency 1000 Hz
3.97

@Frequency 1000 Hz
ASTM D150-98
4.65

@Frequency 60.0 Hz
4.65

@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 14.9 - 15.5 kV/mm
378 - 394 kV/in
ASTM D149-97a
Descriptive Properties Value Comments
Color White