Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Novolen® 3520 L Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Novolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Novolen® 3520 L Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Grade containing antiblocking agent; sealing layer for OPP film.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
Water Absorption 0.10 %
0.10 %
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
Elongation at Break >= 50 %
>= 50 %
Tensile Modulus 0.500 GPa
72.5 ksi
Charpy Impact Unnotched NB
NB
2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
0.200 J/cm²

@Temperature -30.0 °C
0.952 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 185 µm/m-°C

@Temperature 20.0 °C
103 µin/in-°F

@Temperature 68.0 °F
Melting Point 130 °C
266 °F
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C
131 °F
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
Vicat Softening Point 54.0 °C
129 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.3

@Frequency 100 Hz
2.3

@Frequency 100 Hz
2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
Dielectric Strength 140 kV/mm
3560 kV/in
Dissipation Factor 0.000070

@Frequency 100 Hz
0.000070

@Frequency 100 Hz
0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
600 V