Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 - 1.20 J/cm² @Temperature -40.0 - -40.0 °C |
1.43 - 5.71 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 0.750 J/cm² Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.400 - 1.20 J/cm² | 1.90 - 5.71 ft-lb/in² | Average value: 0.670 J/cm² Grade Count:17 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.600 - 1.20 J/cm² | 2.86 - 5.71 ft-lb/in² | Average value: 0.933 J/cm² Grade Count:3 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact, Notched | 0.300 - 1.20 J/cm² @Temperature -40.0 - 0.000 °C |
1.43 - 5.71 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 0.633 J/cm² Grade Count:10 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact, Notched | 0.700 - 1.20 J/cm² | 3.33 - 5.71 ft-lb/in² | Average value: 0.850 J/cm² Grade Count:13 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Charpy Impact, Notched | 0.700 - 1.20 J/cm² | 3.33 - 5.71 ft-lb/in² | Average value: 0.896 J/cm² Grade Count:13 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Charpy Impact, Notched | 0.700 - 1.20 J/cm² | 3.33 - 5.71 ft-lb/in² | Average value: 0.900 J/cm² Grade Count:7 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Charpy Impact, Notched | 0.400 - 1.20 J/cm² | 1.90 - 5.71 ft-lb/in² | Average value: 0.842 J/cm² Grade Count:12 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Charpy Impact, Notched | 0.360 - 1.20 J/cm² | 1.71 - 5.71 ft-lb/in² | Average value: 0.866 J/cm² Grade Count:10 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Charpy Impact, Notched | 0.300 - 1.20 J/cm² | 1.43 - 5.71 ft-lb/in² | Average value: 0.688 J/cm² Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Charpy Impact, Notched | 0.300 - 1.20 J/cm² | 1.43 - 5.71 ft-lb/in² | Average value: 0.730 J/cm² Grade Count:22 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact, Notched | 0.200 - 1.20 J/cm² @Temperature -40.0 - -20.0 °C |
0.952 - 5.71 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.566 J/cm² Grade Count:34 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Charpy Impact, Notched | 0.500 - 1.20 J/cm² | 2.38 - 5.71 ft-lb/in² | Average value: 0.889 J/cm² Grade Count:9 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact, Notched | 1.00 - 1.20 J/cm² | 4.76 - 5.71 ft-lb/in² | Average value: 1.07 J/cm² Grade Count:7 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.200 - 1.20 J/cm² | 0.952 - 5.71 ft-lb/in² | Average value: 0.520 J/cm² Grade Count:16 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Charpy Impact, Notched | 1.20 - 1.20 J/cm² @Temperature -30.0 - -30.0 °C |
5.71 - 5.71 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.20 J/cm² Grade Count:1 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Charpy Impact, Notched | 0.700 - 1.20 J/cm² @Temperature -30.0 - -20.0 °C |
3.33 - 5.71 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.950 J/cm² Grade Count:2 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Charpy Impact, Notched | 0.100 - 1.20 J/cm² @Temperature -30.0 - -20.0 °C |
0.476 - 5.71 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.500 J/cm² Grade Count:5 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Charpy Impact, Notched | 0.300 - 1.20 J/cm² | 1.43 - 5.71 ft-lb/in² | Average value: 0.609 J/cm² Grade Count:19 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.600 - 1.20 J/cm² @Temperature -30.0 - -20.0 °C |
2.86 - 5.71 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.875 J/cm² Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Charpy Impact, Notched | 0.400 - 1.20 J/cm² @Temperature -30.0 - -20.0 °C |
1.90 - 5.71 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.897 J/cm² Grade Count:30 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.800 - 1.20 J/cm² @Temperature -40.0 - -30.0 °C |
3.81 - 5.71 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.945 J/cm² Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Charpy Impact, Notched | 0.340 - 1.20 J/cm² | 1.62 - 5.71 ft-lb/in² | Average value: 0.851 J/cm² Grade Count:14 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Charpy Impact, Notched | 0.400 - 1.20 J/cm² @Temperature -40.0 - -30.0 °C |
1.90 - 5.71 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.850 J/cm² Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Charpy Impact, Notched | 0.200 - 1.20 J/cm² | 0.952 - 5.71 ft-lb/in² | Average value: 0.689 J/cm² Grade Count:8 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 0.600 - 1.20 J/cm² @Temperature -30.0 - 30.0 °C |
2.86 - 5.71 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.843 J/cm² Grade Count:20 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.700 - 1.20 J/cm² @Temperature -30.0 - -20.0 °C |
3.33 - 5.71 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.985 J/cm² Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |