Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179 |
Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 TF-GV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.10 - 7.00 J/cm² @Temperature -40.0 - -30.0 °C |
5.24 - 33.3 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 2.14 J/cm² Grade Count:11 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179 |
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179 |
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
ASTM D256 |
Qualchem Danaprop PP2GF-15 Polypropylene, 15% Glass Fiber Polypropylene (homo-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | DIN 53453 |
Nilit FRIANYL C73 TFGV1530 Nylon 6.6/6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® M305 Grade for smart cards, good dimensional accuracy, excellent dynamic loading capacity.,Property data per ISO test methods. |
|||
Charpy Impact, Notched | >= 1.10 J/cm² @Temperature 23.0 °C |
>= 5.24 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® B1S25 G30PV0 30% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 6 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 545 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 330HR Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 15 HWCP 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179 |
Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-756 ABS - High Flow High rigid, high flow |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | |
Arkema Group Nakan® RPS 400 M PVC, Rigid Extrusion Grade NAKAN RPS 400 M is a rigid polyvinyl chloride compound developed for extrusion of cables ducts.ISO data provided by the manufacturer, Arkema. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BMF Nylon 11 (Dry) Designation ISO 1874-PA11,M,12-010Rigid grade for injection molding. Available color: natural. Additive free.Good melt viscosity. Outstanding ability to mold part with high length-thickness ratio an.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179 |
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Conditioned) Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Charpy Impact, Notched | 1.10 - 4.80 J/cm² | 5.24 - 22.8 ft-lb/in² | Average value: 2.98 J/cm² Grade Count:10 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.24 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |